| Sign In | Join Free | My spintoband.com |
|
Brand Name : Tankii
Model Number : 0cr21al6nb
Place of Origin : China
MOQ : 10kg
Price : 7USD/kg
Payment Terms : D/P,T/T,D/A,L/C,Western Union,MoneyGram
Supply Ability : 1000kg Per Week
Delivery Time : 10-15days
Packaging Details : case
Resistivity : 1.25~1.53 Ω/M
Thermal Conductivity : 46.1 Kj/M.HºC
Maximum Temperature : 1250ºC
Specification : 0.02-7.5mm
Production Capacity : 1000kg Per Week
HS Code : 7506100000
0cr21al6nb Fecral Alloy Ferro Chrome Electric Heating Resistance Wire
1Cr13Al4, 0Cr25Al5, 0Cr23Al5, 0Cr21Al6, 0Cr21Al4, 0Cr21Al6Nb, 0Cr27Al7Mo2 is one kind of normal material of Fe-Cr-Al alloy.
FeCrAl alloy has the characteristic of high resistivity,low temperature resistance coefficient,high operating temperature,goodanti-oxidation and anti-corrosion under high temperature.
It is widely used in industrial furnace, household appliances, industry furnace, metallurgy, machinery, aircraft, automotive,
For other industries producing heating elements and resistance elements.
| Alloy Nomenclature Performance | 1Cr13AL4 | 0Cr25Al5 | 0Cr21AL6 | 0Cr23Al5 | 0Cr21Al4 | 0Cr21Al6Nb | 0Cr27Al7Mo2 | |
| Cr | 12.0-15.0 | 23.0-26.0 | 19.0-22.0 | 20.5-23.5 | 18.0-21.0 | 21.0-23.0 | 26.5-27.8 | |
| Al | 4.0-6.0 | 4.5-6.5 | 5.0-7.0 | 4.2-5.3 | 3.0-4.2 | 5.0-7.0 | 6.0-7.0 | |
| Main Chemical composition | Re | opportune | opportune | opportune | opportune | opportune | opportune | opportune |
| Fe | Rest | Rest | Rest | Rest | Rest | Rest | Rest | |
| Nb0.5 | Mo1.8-2.2 | |||||||
| Max. continuous service temp. of element(ºC) | 950 | 1250 | 1250 | 1250 | 1100 | 1350 | 1400 | |
| Resistivity at 20ºC(μΩ/m) | 1.25 | 1.42 | 1.42 | 1.35 | 1.23 | 1.45 | 1.53 | |
| Density(g/cm3) | 7.4 | 7.1 | 7.16 | 7.25 | 7.35 | 7.1 | 7.1 | |
| Thermal conductivity(KJ/m.h.ºC) | 52.7 | 46.1 | 63.2 | 60.2 | 46.9 | 46.1 | -- | |
| Coefficient of lines expansion(α*10-6/ºC) | 15.4 | 16 | 14.7 | 15 | 13.5 | 16 | 16 | |
| Melting point approx.( ºC) | 1450 | 1500 | 1500 | 1500 | 1500 | 1510 | 1520 | |
| Tensile strength(N/mm2) | 580-680 | 630-780 | 630-780 | 630-780 | 600-700 | 650-800 | 680-830 | |
| Elongation at rupture(%) | >16 | >12 | >12 | >12 | >12 | >12 | >10 | |
| Variation of area(%) | 65-75 | 60-75 | 65-75 | 65-75 | 65-75 | 65-75 | 65-75 | |
| Repeat Bending frequency(F/R) | >5 | >5 | >5 | >5 | >5 | >5 | >5 | |
| Hardness(H.B.) | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | |
| continuous service time(Hours/ ºC) | -- | ≥80/1300 | ≥80/1300 | ≥80/1300 | ≥80/1250 | ≥50/1350 | ≥50/1350 | |
| Micrographic structure | Ferrite | Ferrite | Ferrite | Ferrite | Ferrite | Ferrite | Ferrite | |
| Magnetic properties | Magnetic | Magnetic | Magnetic | Magnetic | Magnetic | Magnetic | Magnetic | |




|
|