Sign In | Join Free | My spintoband.com |
|
Brand Name : TANKII
Model Number : TKN66
Certification : ISO9001 SGS
Place of Origin : Shanghai, China
MOQ : 100 KG
Price : negotiable
Payment Terms : L/C, T/T, Western Union
Supply Ability : 300 Tons per month
Delivery Time : 7-20 days
Packaging Details : Wooned Case
Model NO. : TKN66
Application : Heater element
Nominal Composition : NI 70%
Specification : 0.10-10.00mm
Origin : China
HS Code : 750522
Production Capacity : 300 Ton/Month
resistivity : 1.17
TKN66 is an austenitic nickel-chromium alloy with a maximum operating temperature of 1200°C. This alloy has a low nickel content and a low temperature coefficient of resistivity. It can be used to replace alloys with higher nickel content. If nickel-chromium 80/20 is used for metal sheathed tubular electric heating elements, it can achieve the same service life as nickel-chromium 80/20.
Chemical Composition and Propertes:
Propertes/Grade | TKN66 | |
Main Chemical Composition(%) | Ni | Bal. |
Cr | 21-23 | |
Fe | 8-10 | |
Maximum operating temperature | 1200 | |
Resistivity at 20ºC (μ Ω · m) | 1.17 |
Max Continuous Service Temperature: | 1200ºC |
Resisivity 20ºC: | 1.09 ohm mm2/m |
Density: | 8.4 g/cm3 |
Thermal Conductivity: | 60.3 KJ/m·h·ºC |
Coefficient of Thermal Expansion: | 18 α×10-6/ºC |
Melting Point: | 1400ºC |
Elongation: | Min 20% |
Micrographic Structure: | Austenite |
Magnetic Property: | nonmagnetic |
Temperature Factors Of Electrical Resistivity
20ºC | 100ºC | 200ºC | 300ºC | 400ºC | 500ºC | 600ºC |
1 | 1.006 | 1.012 | 1.018 | 1.025 | 1.026 | 1.018 |
700ºC | 800ºC | 900ºC | 1000ºC | 1100ºC | 1200ºC | 1300ºC |
1.01 | 1.008 | 1.01 | 1.014 | 1.021 | 1.025 | - |
Chemical Composition and Main Properties of Nichrome wire | ||||||
Properties Grade | NiCr 80/20 | NiCr 70/30 | NiCr 60/15 | NiCr 35/20 | NiCr 30/20 | |
Main Chemical Composition | Ni | Balance | Balance | 55.0-61.0 | 34.0-37.0 | 30.0-34.0 |
Cr | 20.0-23.0 | 28.0-31.0 | 15.0-18.0 | 18.0-21.0 | 18.0-21.0 | |
Fe | ≤ 1.0 | ≤ 1.0 | Balance | Balance | Balance | |
Max Continuous Service Temperature(oC) | 1200 | 1250 | 1150 | 1100 | 1100 | |
Resisivity 20oC (Ω mm2/m) | 1.09 | 1.18 | 1.12 | 1.04 | 1.04 | |
Density (g/cm3) | 8.4 | 8.1 | 8.2 | 7.9 | 7.9 | |
Thermal Conductivity(KJ/m@ h@ oC) | 60.3 | 45.2 | 45.2 | 43.8 | 43.8 | |
Coefficient of Thermal Expansion(α × 10-6/oC) | 18 | 17 | 17 | 19 | 19 | |
Melting Point( oC) | 1400 | 1380 | 1390 | 1390 | 1390 | |
Elongation(%) | > 20 | > 20 | > 20 | > 20 | > 20 | |
Micrographic Structure | austenite | austenite | austenite | austenite | austenite | |
Magnetic Property | nonmagnetic | nonmagnetic | nonmagnetic | Weak magnetic | Weak |
![]() |